如何解决纸箱出现坍塌的现象?

来源:http://www.shuangfengbaozhuang.cn 时间:2020-05-13

  在生产过程中会遇到一个头疼的问题,就是纸箱的坍塌和粘胶箱机不牢固的问题,总结出的解决办法就是提高纸板的材质,提高抗压强度和防潮性能,从而降坍塌率。另外,工厂需要提高粘接强度,增加淀粉糊的固含量,通过减少胶水的用量来提高纸板的硬度,解决了粘盒机的问题。
  In the process of production, there will be a headache, that is, the collapse of the carton and the unsteadiness of the viscose box machine. The solution summed up is to improve the material quality of the cardboard, improve the compressive strength and moisture-proof performance, so as to reduce the collapse rate. In addition, the factory needs to improve the bonding strength, increase the solid content of starch paste, improve the hardness of cardboard by reducing the amount of glue, and solve the problem of box gluing machine.
  包装厂如何处理粘盒机不牢固盒坍塌的问题生产使用时应注意以下几点:
  How to deal with the collapse of the loose box of the box gluing machine in the packaging factory should pay attention to the following points in production and use:
  1、控制生纸的使用
  1. Control the use of raw paper
  检查瓦楞纸的施胶状况、原纸表面吸水指数的效能。如果原始纸张的表面施胶差,吸水会偏高,而且很容易受温冷藏和潮湿环境,导致的水分,软化并减少完成的抗压强度。
  Check the sizing condition of corrugated paper and the efficiency of water absorption index of base paper surface. If the surface sizing of the original paper is poor, the water absorption will be high, and it is easy to suffer from low temperature cold storage and humid environment, resulting in moisture, softening and reducing the finished compressive strength.
纸箱厂家
  2、生产纸板要控制纸板的含水量
  2. To control the moisture content of paperboard in production
  纸板的含水率不能太多,因为含水率是纸板硬度,影响纸板的边压指数。在纸板加工过程中,单面机和双面机的上胶量不能太大。一旦胶水量大,纸板的形状就会变形,而瓦楞纸板的形状则直接影响纸板的边压、边压,抗压强度也会降。
  The moisture content of the paperboard can not be too much, because the moisture content is the low hardness of the paperboard, which affects the edge pressure index of the paperboard. In the process of cardboard processing, the amount of glue on single-sided machine and double-sided machine should not be too large. Once the amount of glue is large, the shape of paperboard will be deformed, while the shape of corrugated paperboard will directly affect the side pressure and side pressure of paperboard, and the compressive strength will also be reduced.
  3、板材的粘接强度要大
  3. The bonding strength of the plate should be large
  粘接强度是瓦楞纸与衬纸、面纸的粘接力。如果纸板假粘着、受压,表面的纸张或纸张会与瓦楞纸分离,那么抗压强度就会直线下降。4. 生产过程中的间隙压力控制要适度
  The adhesive strength is the adhesive force between corrugated paper, liner paper and surface paper. If the paperboard is stuck and pressed, the surface paper or paper will be separated from the corrugated paper, then the compressive strength will drop in a straight line. 4. The gap pressure control in the production process should be moderate
  特别要注意的是,糊盒机的糊料间隙压力不能太小,双面机、模切机的太阳轮的间隙压力要控制在合理的范围内,以避免瓦楞坍塌,影响纸板的抗压强度。
  In particular, the paste gap pressure of the pasting machine should not be too small, and the gap pressure of the sun wheel of the double-sided machine and the die-cutting machine should be controlled within a reasonable range to avoid the corrugation collapse and affect the compressive strength of the cardboard.
  5、采用喷淋剂、防水轻油等表面解决防水防潮问题
  5. Using spray agent, waterproof light oil and other surfaces to solve the problem of waterproof and moisture-proof